日本宇部 PA12 3035JL1塑料原料 宇部
日本宇部 PA12 3035JL1塑料原料 宇部
3035JL1
聚十二内酰胺#尼龙12|PA12
日本宇部
物性信息:
成型收缩率 | |||
(UBEmetho) | 0.7 | % | |
1.8 | % | UBEmethod | |
吸水率 | ASTM D-570 | ||
1.4 | % | ||
0.20 | % |
比重 | 1.03 | ASTM D-792 |
弯曲强度 (80°) | 110 | kgf/cm | ASTM D-790 |
屈服下的伸张强度 (-30°) | 670 | kgf/cm | ASTM D-638 |
抗冲击强度 (-30°) | 5.0 | kgf.cm/cm | ASTM D-256 |
断裂下的伸张强度 (23°) | >410 | kgf/cm | ASTM D-638 |
屈服下的伸张强度 (23°) | 250 | kgf/cm | ASTM D-638 |
断裂下的伸张强度 (23°) | >440 | kgf/cm | ASTM D-638 |
Taber磨耗率 | 7 | mg | ASTM D-1044 |
屈服下的伸张强度 (23°) | 270 | kgf/cm | ASTM D-638 |
剪切强度 (23°) | 250 | kgf/cm | ASTM D-732 |
弯曲弹性率 | ASTM D-790 | ||
(23°) | 4200 | kgf/cm | |
(23°) | 4000 | kgf/cm | |
弯曲强度 (-30°) | 900 | kgf/cm | ASTM D-790 |
屈服下的伸张强度 (80°) | 120 | kgf/cm | ASTM D-638 |
弯曲强度 (23°) | 180 | kgf/cm | ASTM D-790 |
抗冲击强度 (23°) | 30 | kgf.cm/cm | ASTM D-256 |
弯曲弹性率 (-30°) | 22500 | kgf/cm | ASTM D-790 |
弯曲强度 (23°) | 200 | kgf/cm | ASTM D-790 |
断裂下的延伸率 (23°) | >300 | % | ASTM D-638 |
弯曲弹性率 (80°) | 2200 | kgf/cm | ASTM D-790 |
硬度(洛氏.布氏) (23°) | 80 | ASTM D-785 |
介电常数 (60HZ) | 11.8 | ASTM D-150 | |
绝缘耐力 | 28 | KV/mm | ASTM D-149 |
介电常数 | ASTM D-150 | ||
(10HZ) | 8.3 | ||
(10HZ) | 3.5 | ||
介电损耗 (10HZ) | 0.11 | ASTM D-150 | |
体积电阻率 | 10 | Ω.cm | ASTM D-257 |
介电损耗 | ASTM D-150 | ||
(60HZ) | 0.14 | ||
(10HZ) | 0.21 |
燃烧率 | HB | UL-94 | |
线性热膨胀系数 | 12 | X的10-5cm/cm/°C | ASTM D-696 |
热变形温度 (4.6kgf/cm) | 135 | °C | ASTM D-648 |
熔点 (DSC) | 166-170 | °C |
发布时间:2024-11-14
展开全文
其他新闻
- 德国科思创 PBT Makroblend KU2-7912/4 2024-11-14
- 瑞士EMS PA66 AZ3/2塑料原料 瑞士EMS 2024-11-14
- 德国朗盛 PBT POCAN B 1305 000000工程塑料 2024-11-14
- 沙伯基础 Sabic PEEK -- THERMOCOMP LC003E 2024-11-14
- 台湾晋伦 PA66 6/Mapex AN2320SB 高耐热 2024-11-14
- 日本可乐丽 PA9T G2330 BK塑胶颗粒 可乐丽 2024-11-14
- 荷兰-- PA46 TE363塑料粒子 荷兰-- 尼龙46 2024-11-14
- 阿科玛 Arkema PA11 BZM 8 TL塑胶料 阿科玛 Arkema 2024-11-14
- 阿科玛 Arkema PA12 AZM 30树脂 阿科玛 Arkema 2024-11-14
- 日本东丽 PA6 CM1026 东丽 PA6 CM1026 2024-11-14