美国Santoprene:TPV 281-64MED、281-73MED、 它的设计适用于需要良好的弹性,外观及密封特性。这品位Vyram冠捷是剪切依赖,可以在常规的热塑性塑料加工设备,注塑,挤出或吹塑。这是聚烯烃基础和完全回收。具有优异的耐温性,耐老化性(耐紫外线和臭氧),与聚烯烃有优异的粘结性能,压缩变形性小等特点,该材料橡胶感强,电性能优异,着色性好,具有优异的抗动态疲劳性,很高的抗撕裂性这种材料结合良好的物理性能和耐化学性,用于广泛的注塑成型应用。这种等级的热塑性冠捷是剪切依赖,并能使用常规的热塑性塑料注塑成型设备。TPV是一系列高性能热塑性弹性体的理想相结合的特点,硫化橡胶,如灵活性和低压缩,与热塑性塑料加工方便。拟合进入中程成本和性能的频谱都热塑性和热固性橡胶,热塑性冠捷接受范围广泛的工业和消费产品应用,热塑性热塑性弹性体具有良好的耐挠曲削减增长,同时,高撕裂强度和极好的抗疲劳,和良好的抗许多酸,碱和水的解决办法。

ExxonMobil Santoprene® 281-64MED Thermoplastic Elastomer

Thermoplastic Vulcanizate Elastomer (TPV)

Exxon Chemical

产品说明:

A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. Prior to release, each medical grade lot undergoes a Cytotoxicity study using the ISO elution method and a Physico-Chemical - Elastomeric Closures test for heavy metals such as lead. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.

Information provided by Advanced Elastomer Systems


物性信息:

物理性能额定值 (公制)额定值 (英制)测试方法
比重0.970 g/cc0.970 g/cc23°C; ASTM D792
机械性能额定值 (公制)额定值 (英制)测试方法
肖氏硬度 (邵氏 A)6464.12 in; ASTM D2240
抗张强度(断裂)6.420 MPa931.2 psiAir at 212°F, 168 hr; ASTM D573

6.69 MPa970 psiAcross Flow; ASTM D412
极限抗拉强度2.48 MPa360 psiAcross Flow; ASTM D412
伸长率 (断裂)482.3 %482.3 %Air at 212°F, 168 hr; ASTM D573

530 %530 %Across Flow; ASTM D412
撕裂强度9.99 kN/m57.0 pli212°F, Die C; ASTM D624

24.0 kN/m137 pli73°F, Die C; ASTM D624
**压缩22 %22 %73°F, 168 hr; ASTM D395

54 %54 %212°F, 168 hr; ASTM D395
加工性能额定值 (公制)额定值 (英制)测试方法
加工温度175 - 230 °C347 - 446 °F
材料描述
测试方法